Hydrogen peroxide bleaching of cellulose pulps obtained from brewer’s spent grain

Author(s): Mussatto, Solange I. cv logo 1 ; Rocha, George J. M. cv logo 2 ; Roberto, Inês Conceição cv logo 3

Date: 2008

Persistent ID: http://hdl.handle.net/1822/8131

Origin: RepositóriUM - Universidade do Minho

Subject(s): Bleaching; Brewer’s spent grain; Cellulose; Hydrogen peroxide; Pulp


Description
Brewer’s spent grain (BSG) was evaluated for bleached pulp production. Two cellulose pulps with different chemical compositionswere produced by soda pulping: one from the original raw material and the other from material pretreated by dilute acid. Both of them were bleached by a totally chlorine-free sequence performed in three stages, using 5% hydrogen peroxide in the two initial, and a 0.25 NNaOHsolution in the last one. Chemical composition, kappa number, viscosity, brightness and yield of bleached and unbleached pulps were evaluated. The high hemicellulose (28.4% w/w) and extractives (5.8% w/w) contents in original BSG affected the pulping and bleaching processes.However, soda pulping of acid pretreated BSG gave a celluloserich pulp (90.4% w/w) with low hemicellulose and extractives contents (7.9% w/w and <3.4% w/w, respectively), which was easily bleached achieving a kappa number of 11.21, viscosity of 3.12 cp, brightness of 71.3%, cellulose content of 95.7% w/w, and residual lignin of 3.4% w/w. Alkaline and oxidative delignification of acid pretreated BSG was found as an attractive approach for producing high-purity, chlorine-free cellulose pulp.
Document Type Article
Language English
delicious logo  facebook logo  linkedin logo  twitter logo 
degois logo
mendeley logo

Related documents



    Financiadores do RCAAP

Fundação para a Ciência e a Tecnologia Universidade do Minho   Governo Português Ministério da Educação e Ciência Programa Operacional da Sociedade do Conhecimento EU