Friction and wear behaviours of Ti(C,O,N) dark decorative coatings

Author(s): Munteanu, D. cv logo 1 ; Gabor, C. cv logo 2 ; Constantin, D. G. cv logo 3 ; Varga, B. cv logo 4 ; Adochite, R. cv logo 5 ; Andrei, O. C. cv logo 6 ; Chappé, J. M. cv logo 7 ; Cunha, L. cv logo 8 ; Moura, C. cv logo 9 ; Vaz, F. cv logo 10

Date: 2011

Persistent ID: http://hdl.handle.net/1822/13480

Origin: RepositóriUM - Universidade do Minho

Subject(s): Decorative coating; Composition; Friction; Wear


Description
Reactive magnetron sputtering was used to obtain dark Ti(C,O,N) decorative coatings onto high speed steel. From a crystallographic point of view, depending by the amount of (N+O) mixture, the obtained films could be divided in two major regions: the first one with a predominant fcc crystallographic structure (for low amounts of (N+O)), and the second one containing films with amorphous structures. The best results for friction coefficient and wear rates (the minimum values) were registered for samples prepared in the beginning of the amorphous region. These two tribological parameters are mainly influenced by the carbon content in the films. Taking into account the practical goal of these kinds of films, the pure black films were obtained for higher amount of (N+O) mixture. Also for these amorphous darkest films reached in oxygen and nitrogen, the tribological properties are acceptable and the adherence reaches the maximum value.
Document Type Article
Language English
delicious logo  facebook logo  linkedin logo  twitter logo 
degois logo
mendeley logo

Related documents



    Financiadores do RCAAP

Fundação para a Ciência e a Tecnologia Universidade do Minho   Governo Português Ministério da Educação e Ciência Programa Operacional da Sociedade do Conhecimento EU