Interest in soil contamination has been growing in recent years due to the ongoing degradation of soil environments. Therefore, the development of remediation techniques and the study of contaminant sorption and migration are areas of intense research. In this study, the authors sought to evaluate the scenario of co-contamination of a loamy sand soil by multiple heavy metals. To that end, the sorption and trans...
The continuous and growing degradation of the environment, due to several anthropogenic activities, is a main concern of the scientific community. Consequently, the development of low cost techniques to clean air, water and soils are under intense investigation. In this study, the focused problem is the soil contamination by hexavalent chromium, which is known for its several industrial applications - productio...
A systematic study of synthesis of different chemical composition of alloys within the quaternary Fe-Si-Ca-Al system, versus acid leaching refining using HCl with or without FeCl3 has been undertaken. Such study has the aim of achieving an adequate structural composition of Fe-Si alloys, in order to obtain high purity and fine particle size silicon by acid leaching, at more reduced costs. The experimental resul...
O silício de grau metalúrgico (% Si> 98%) é a matéria-prima habitualmente utilizada para a produção de silício de elevado grau de pureza (99,9% de Si). As principais impurezas metálicas são o ferro, o alumínio e o cálcio. Estas impurezas têm elevados coeficientes de segregação no silício: as suas solubilidades são grandes no silício fundido mas pequenas na fase sólida. Portanto, as fases que contêm as impurezas...
Silicon with high purity and fine particle size can be produced by acid leaching of Fe-Si industrial alloys under the condition that they have adequate chemical composition and structural constitution. Such alloys contain phases that fall within the system Fe-Si-Ca-Al, where the quaternary phase Caalsifer, with aproximate formula (Fe0.8Al0.1 0.1) (Si0.8Ca0.2)2, is found along with several binary and ternary pha...
A maior parte dos estudos cinéticos de solubilização do ferro em meios ácidos clorídricos [1-7] foram realizados na ausência de oxigénio. Neste trabalho estudou-se a influência dos iões H+, Cl- e Fe3+ na corrosão de um ferro em meio arejado, utilizando a técnica LSV ("Linear Sweep Voltammetry". Os dados experimentais obtidos, corrente/potencial, permitem determinar as densidades de corrente de corrosão, assim c...
A dissolução anódica do ferro foi estudada em meio de ácido clorídrico (força iónica constante de 4,0 M) usando voltametria linear (velocidade de varrimento = 2mV/s), a 25ºC, na presença e na ausência de ião férrico. A dissolução do ferro é acelerada quer pelos iões H+ quer pelos iões Cl, na gama de concentrações estudada. O ião férrico inibe a dissolução do ferro entre 0,025M e 0,1 M e acelera o processo entr...