There are a number of distinguishable carbide phases in the binary Mo-C system depending on C/Mo ratio as well as on temperature. In a preceding work published in this journal, carbide formation performance for graphite/molybdenum powder mixtures at specified levels of substoichiometric C/Mo atom ratio (C/Mo = 1/1, 3/4, 2/3 and 1/2) by exposure to concentrated solar radiation in a solar furnace at PROMESCNRS in...
In equilibrium binary W-C system, mono-carbide WC is acknowledged as the stable phase under presence of excess free carbon up to temperature 2700 C whereas sub-carbideW2C would form between 1250 C and 2700 C under the carbon-deficiency condition. In unique setup of solar furnace at PROMES-CNRS in Odeillo (France), temperature of specimen is raised from the ambient temperature to target temperature up to 2000 C ...