Thermal degradation of as electrospun chitosan membranes and samples subsequently treated with ethanol and cross-linked with glutaraldehyde (GA) have been studied by thermogravimetry (TG) coupled with an infrared spectrometer (FTIR). The influence of the electrospinning process and cross-linking in the electrospun chitosan thermal stability was evaluated. Up to three degradation steps were observed in the TG da...
Fiber meshes of poly(hydroxybutyrate) (PHB) and poly(hydroxybutyrate)/ poly(ethylene oxide) (PHB/PEO) with different concentrations of chlorhexidine (CHX) were prepared by electrospinning, for assessment as a polymer based drug delivery system. The electrospun fibers were characterized at morphological, molecular and mechanical levels. The bactericidal potential of PHB and PHB/PEO electrospun fibers with and wi...
Poly(vinylidene fluoride) electrospun membranes have been prepared with different NaY zeolite contents up to 32%wt. Inclusion of zeolites induces an increase of average fiber size from ~200 nm in the pure polymer up to ~500 nm in the composite with 16%wt zeolite content. For higher filler contents, a wider distribution of fibers occurs leading to a broader size distributions between the previous fiber size valu...
Avaliou-se a ocorrência de distúrbios na coagulação plasmática e na plaquetometria de cães infectados por Ehrlichia spp., durante 15 semanas após o contágio. Doze cães, entre machos e fêmeas, nascidos em estação experimental e com idades entre um e dois anos, foram usados no experimento. Nove cães foram infectados experimentalmente com sangue de cão naturalmente portador de Ehrlichia spp. e três foram mantidos ...
Metodologia. Caracterização de Pseudomonas fluorescentes. Caracterização genotípica por análise da região ITS1. ; 2005
Financiadores do RCAAP | |||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |