The relaxation of the initial magnetic permeability of La doped yttrium iron garnet (YIG) samples with nominal composition Y3-xLaxFe5O12 (0< x <0.6) is analysed in this work. The results show a very different behaviour depending on the sintering atmosphere used for the fabrication of the samples. Concretely, for the samples sintered in air, it just have been detected the usual relaxation peak found in YIG at 13...